Understanding and Controlling Atomic Layer Deposition of Platinum and Platinum Oxide
- Author
- Ivo Erkens
- Year
- 2014
- Abstract & Cover
- Source of Information
- Harm Knoops
- University
- Eindhoven University of Technology (Eindhoven, Netherlands)
- External Link
- Read Thesis
Atomic layer deposition (ALD) is a thin-film deposition technique, yielding high quality thin-film materials with precise thickness control, excellent uniformity over large-area substrates, and superior conformality over demanding 3-D topologies. The standard ALD approach is thermally activated growth using two or more self-limiting half-reactions. Novel technology options arise by going beyond this standard, such as e.g. plasma-assisted deposition enabling low substrate temperatures, the deposition of nanoparticles, or the deposition of doped materials. This makes ALD a promising technique in emerging applications using heterogeneous device integration in the so-called More than Moore domain. Pt and PtOx are relevant materials in these new application fields, with many potential uses for both thin films and nanoparticles deposited on planar substrates as well as on challenging surface topologies. In this dissertation, the process windows of Pt and PtOx layer growth by ALD from (MeCp)PtMe3 vapor and O2 gas/plasma have been explored and expanded using both planar and 3D substrates. First, the reaction mechanism of the thermal Pt ALD process was elucidated by studying the volatile reaction products during the precursor and oxygen step using in situ mass spectrometry. This showed that the lower limit of the temperature window (250-300 °C) is determined by the accumulation of carbonaceous surface species at the Pt surface thus inhibiting the dissociation of oxygen molecules. When using an O2 plasma instead of O2 gas, O-radicals are created and supplied directly from the gas phase to the surface. The O-radicals make surface-mediated dissociation no longer necessary and enable the combustion of the carbonaceous surface species at much lower temperatures, thus extending the lower limit of the temperature window down to room temperature. The composition of the deposited films for the plasma-assisted ALD process based on (MeCp)PtMe3 and O2 plasma was found to be governed by three main parameters: the substrate temperature, the O2 plasma exposure, and the (MeCp)PtMe3 precursor exposure. By an extensive investigation of the influence of these three parameters, we succeeded in adding PtOx to the ALD materials toolbox. It has been established that with increasing substrate temperature, the thermal stability of PtOx decreases and the reducing activity of the precursor ligands increases. Therefore, longer O2 plasma exposures and/or lower (MeCp)PtMe3 exposures are required to obtain PtOx at higher temperatures. Finally, it was shown that both PtOx nanoparticles and ultrathin films can be deposited in a temperature window ranging from room temperature to 300 °C. For the conformal deposition of thin films of Pt and PtOx in high aspect ratio (HAR) features, the (MeCp)PtMe3 vapor and O2 plasma exposures need to be carefully chosen in order to ensure that the surface reactions are saturated throughout the feature. It was demonstrated that Pt-films can be deposited conformally in trenches with an aspect ratio of up to 34. Films of PtOx were deposited conformally in trenches with an aspect ratio of up to 9. Remarkably, by tuning the substrate temperature, and precursor and O2 plasma exposure, both Pt and PtOx can be deposited concurrently in a single HAR feature. In this case, even the composition profile along the feature can be explained and controlled. Furthermore, an example of how ALD of Pt can be applied in future applications was given. Gas sensing structures prepared from Al-doped ZnO layers were coated with catalytic ALD-Pt nanoparticles. It was demonstrated how this paves the way for room temperature detection of O2 (down to 0.5 % O2 in N2) and CO (down to 20 ppm CO in N2). Room temperature gas detection would make the necessary heating element in today’s gas sensing devices obsolete, and thus open up pathways for the further reduction or ultimately the elimination of heating power for ultralow power (< 100 μW) ZnO-based sensing devices used in wireless autonomous sensing networks. In summary, the work presented in this dissertation has led to a better understanding of ALD of both Pt and PtOx . The insights that were obtained at the atomic level enable an extremely accurate degree of materials and process control required for future applications in electronics and other fields. It is this level of control that allows the properties of ALD-grown layers of Pt and PtOx to be tailored to the envisioned next-generation More than Moore-type devices.