Growth and Leakage Current Control of High-k SrTiO3 Thin Films Grown via Atomic Layer Deposition

Author
Sang Hyeon Kim
Year
2019
Abstract & Cover

A DRAM cell consists of one capacitor and one transistor. In a DRAM cell, a transistor plays a role of selecting a cell to be read or written in a DRAM cell array, and a capacitor stores charges to record '0' and '1' data. In order to integrate DRAM devices, it is essential to develop various process element technologies including transistors and capacitors. Among them, capacitor element technology is a crucial technology for ensuring sufficient capacitance in a small area. The currently produced DRAM has a sandwich structure (ZAZ) with ZrO2-based Al2O3 as a high-k film. This thesis reported the growth behavior, the low-temperature deposition method and the leakage current reduction of the high-k SrTiO3 (STO) by atomic layer deposition. In this thesis, Sr(i PrCp)2 and Ti(OMe)3(CpMe5) were used with strontium precursor and titanium precursor with ozone and water as an oxygen source, respectively. The growth behavior of the STO thin film deposition process was studied, and various thin film characteristics such as electrical characteristics analysis through the fabrication of metal-insulator-metal (MIM) structure capacitors were also evaluated. First, the growth behavior of the upper thin film of the STO thin films deposited in two stages was studied. The annealing temperature of the 5 nm thick underlayer deposited on amorphous phase was varied from 450 to 650 °C to vary the crystallinity of the underlayer. The crystallization and growth behavior of the upper thin film was analyzed without depositing the upper thin film deposited at 650 °C at a high temperature. Amorphous and crystalline materials were mixed at a crystallization temperature of 550 °C to 600 °C, and the deposited thin film also depends on the crystallinity of the underlying thin film. Further, when Ru is deposited as a lower substrate, oxygen is diffused between the crystal grains of the lower STO thin film, and the growth rate of the upper STO thin film is increased. This excessive oxygen supply phenomenon does not occur when silicon is used as the lower substrate. When the heat treatment temperature of the lower STO thin film is higher than 600 °C, almost all of the lower STO thin film is heat treated, and the upper STO thin film is also crystallized with the same tendency. As a result, an equivalent oxide film of 0.52 nm was formed at a leakage current of 2.5×10-8 A/cm2 Second, the deposition temperature of the lower STO thin film was deposited at a low temperature of 230 °C. Moreover, the upper STO thin film was deposited at a high temperature of 370 °C. The STO thin film has high leakage current characteristics associated with low band gap energy and ruthenium metal having a high work function as the electrode material should be applied in order to lower the leakage current. However, reactions that are similar to chemical vapor reactions occur at ruthenium and STO interfaces with unreasonably high reactivity. This high reactivity is because the ruthenium undergoes redox process and supplies excess oxygen to the strontium oxide film having a considerable thermodynamic forming energy. The deposition temperature was lowered by annealing at a low temperature of 230 °C, suppressing the abnormal reaction, and the microcracks of the lower STO thin film were reduced to form a denser lower STO thin film and increase the density of the STO thin film deposited on the upper side. As a result, the bulk dielectric constant increased from 101 to 167 under the conditions of deposition of the lower STO thin film at a high temperature of 370 °C. However, there is a disadvantage in that the carbon doping increases and the thickness of the equivalent oxide film at the interface increase as the deposition time increases at the low-temperature deposition. Third, Al was doped to reduce the high leakage current of STO thin films with low bandgap energies of 3.0 to 3.2 electron volts. One cycle of Al oxide was doped into the STO thin film, and the Al doping positions were evaluated between the lower STO thin film and the ruthenium substrate and at the top of the upper STO thin film. When the bottom Al is doped, crystallization of the lower STO thin film is lowered, and the dielectric constant of the upper STO thin film is lowered from 149 to 71. When the uppermost STO thin film is doped with Al, crystallinity of the crystallized STO thin film is not significantly affected. However, in both cases, the decrease in leakage current is more than 20 times, which is a result of improvement in the relationship between the leakage current density and the equivalent oxide film. As a result, the thickness of the equivalent oxide film at 0.8 volt, which is the operating voltage of the DRAM, decreases from 0.71 nm to 0.63 nm, and the physical thickness also decreases from 10.3 nm to 8.6 nm. In conclusion the behavior of the STO thin film deposited on the Ru electrode in two steps was analyzed to analyze the crystalline and amorphous growth behavior at the critical temperature, and the deposition temperature was lowered to suppress the non-ideal deposition phenomenon. In order to overcome the low band-gap energy of the STO film, Al was doped to reduce the tox to 0.63 nm and the tphy to 8.6 nm at the operating voltage of 0.8V.

Source of Information
Cheol Seong Hwang
University
Seoul National University
(Seoul, Korea)
Other notes
http://dcollection.snu.ac.kr/common/orgView/000000153980
Read Thesis
LinkedIn
linkedin invite