Gas Diffusion Barriers Using Atomic Layer Deposition: A New Calcium Test and Polymer Substrate Effects

Author
Jacob Andrew Bertrand
Year
2012
Abstract & Cover

The increasing demand on available energy resources has led to a desire for  more energy efficient devices. The wide use of displays in consumer electronics, such as  televisions, cell phones, cameras and computers makes them an ideal target for improvement.  Organic light-emitting diodes (OLEDs) are a good candidate to replace traditional Si based  devices. However, the low work function metals typically used as electrodes in OLEDs are very  reactive with water and oxygen. Ultralow permeability gas diffusion barriers with water vapor  transmission rates (WVTRs) as low as <10-6 g/(m2*day) are required on the polymers used to  fabricate organic electronic and thin film photovoltaic devices.  Atomic Layer Deposition (ALD) uses self-limiting surface reactions to deposit thin  conformal films. ALD is capable of depositing thin, conformal, high quality barriers. WVTR  values as low as  5 x 10-5 g/(m2*day) have been measured for Al2O3 ALD films at 38C/85% RH  using the Ca test with optical transmission probing. The Ca test is a technique with very high  sensitivity to measure ultralow WVTRs. This test relies on measuring the oxidation of a Ca  metal film by monitoring the change in its optical or electrical properties. However, glass lid  control experiments have indicated that the WVTRs measured by the Ca test are limited by H2O  permeability through the epoxy seals. Varying results have been reported in the literature  using the electrical conductance of Ca to measure permeation. In this work, two approaches were applied to overcome the epoxy edge seal limitations.  The first approach was to deposit Al2O3 ALD barriers directly on Ca metal. While the Al2O3 ALD  barriers were successfully deposited, the measurement of an accurate WVTR was limited by  barrier pinholes. The presence of pinholes in the Al2O3 ALD barrier on Ca results in the localized  oxidation of the Ca sensor. Heterogeneous degradation of the Ca causes inaccuracies in the  conductance of the film. As oxidation regions merge, large percolation paths are severed  without complete Ca oxidation. To solve this problem, a new apparatus was developed that  measures the electrical conductance of Ca films. This new apparatus does not rely on epoxy  seals and separates the Ca metal from the barrier. Unfortunately, the electrical conductance of  the Ca film versus Ca oxidation was found to be extremely nonlinear. This nonlinearity severely  complicates the usual analysis to obtain WVTR values from the Ca test.  The new apparatus was useful for the examination of PEN polymer substrates using the  total lifetime of the Ca sensor. Polymer effects on the measurement of gas permeability for  polymer/barrier systems have largely been ignored. Experiments were performed to determine  the effect of the PEN polymer substrates on the WVTR measurement. The H2O permeation  activation energy in the PEN polymer, the effect of water saturation of the PEN polymer and  the dependence of the lifetime of the Ca sensor on the H2O flux on the PEN substrate were of  particular interest. The experiments obtained H2O permeation activation energies in the PEN  polymer of 12.4 kJ/mol. The Ca sensor lifetime was found to be linear with H2O flux. No  difference in Ca sensor lifetime was observed between dry or H2O-saturated PEN polymer  substrates.  

Source of Information
http://libraries.colorado.edu/record=b7463195~S3
University
University of Colorado Boulder
(Boulder, USA)
Read Thesis
LinkedIn
linkedin invite